MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Phillips 66 SynXPA® HC-150 H Lubricant HC-150
Categories: Fluid; Lubricant; Synthetic Ether Base

Material Notes: Description: Conoco SynXPA H Lubricant is a premium-quality synthetic-polyolester lubricant that offers protection for heavily loaded and partially opened open gears, such as those in ball mills, shovels, kilns and draglines. It is also useful for wire ropes, shovel boom sticks and slow moving bearings. It is inherently biodegradable (up to 90 percent biodegradable, as per CEC, OECD testing) and nontoxic (As per acute mammalian toxicity studies.). SynXPA H Lubricant can be applied to the surface through most automatic lubricators or through automated delivery lines and an air assisted sprayer. Pressure-lubrication bins, lines and pumps need not be purged unless they are plugged by residual asphaltic materials. SynXPA H Lubricant meets the performance requirements of the American Gear Manufacturers Association (AGMA) 251.02 Specification for high-viscosity-grade, extreme-pressure gear lubricants. SynXPA H Lubricant offers high film strength and film thickness. It spreads out and coats surfaces evenly for better distribution of load. It reduces the gear surface temperatures and minimizes the temperature gradient across the gear face, which typically is associated with slightly misaligned gear sets. Polyolesters have great affinity for metals. As such, SynXPA H Lubricant bonds to gear surfaces and provides exceptional shock loading protection at startups and in situations where the equipment may be idle for extended periods of time.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Kinematic Viscosity at 40°C (104°F) 3400 cSt
Kinematic Viscosity at 100°C (212°F) 260 cSt
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Load Wear Index 126
Four Ball Extreme Pressure, Weld Load 500 kg
Four Ball Wear 1.01 mm
Penetration 310 - 340ASTM D-217
Timken Test 60.0 lb
 
Thermal PropertiesOriginal ValueComments
Flash Point 220 °F
 
Descriptive Properties
ColorBrown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tipco Tipcolite® THD 121 Phenolic Compound, Wood Flour, having Medium Flow & High Strength
Magnesium Elektron Elektron® 43 Magnesium Extrusion Alloy, UNS M18434
Bamberger Polymers Bapolan® ABS8430 ABS Polymer, Extrusion/Injection Grade
Arkema Rilsamid® AESNO 14 TL PA12
Arkema Rilsamid® AESN BLACK P401 TL PA12

WCON185 / 75222

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.