MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Crosspolimeri POLIGOM G/42 EPR/HEPR/EPDM
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: POLIGOMN: is the trade mark of our crosslinkable EPR/HEPR/EPDM compound ( phthalate plasticizers free ).

POLIGOM G/42: halogen free chemically crosslinkable elastomer for low voltage cable insulation and sheathing: suitable for G7. It is a conveniently grafted compound able to react in presence of moisture and of a catalyst. We normally suggest our catalyst type MAC/400 PS or MAC/100 SCU (more reactive). FOR SOLAR CABLES INSULATION WE SUGGEST TO USE CATALYST MAC/520 PSL at 7/10%. REACTION BETWEEN GRAFTING AND CATALYST: These two compounds, separately stored, must be mixed before starting extrusion in the ratio: GRAFTING/CATALYST 94/6

Certify: EN 50363- G7, BS7655 GP4-GP5-GP6-GP7, CEI 2011 G7, EN 50620 EVI-2, IEC 60502 EPR-HEPR

Information provided by Crosspolimeri S.P.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.890 g/cc0.890 g/ccASTM D792
Melt Flow 4.0 - 6.0 g/10 min
@Load 5.00 kg,
Temperature 190 °C
4.0 - 6.0 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Storage Temperature 12.0 °C53.6 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9090ASTM D2240
Tensile Strength >= 18.0 MPa>= 2610 psiIEC 60811
 >= 180.72 MPa
@Temperature 127 °C,
Time 144000 sec
>= 26211 psi
@Temperature 261 °F,
Time 40.0 hour
Air bomb; IEC 60811
 >= 181.26 MPa
@Temperature 150 °C,
Time 605000 sec
>= 26290 psi
@Temperature 302 °F,
Time 168 hour
Heat Ageing; IEC 60811
Elongation at Break >= 450 %>= 450 %IEC 60811
 >= 405 %
@Temperature 150 °C,
Time 605000 sec
>= 405 %
@Temperature 302 °F,
Time 168 hour
Heat Ageing; IEC 60811
 >= 463.5 %
@Temperature 127 °C,
Time 144000 sec
>= 463.5 %
@Temperature 261 °F,
Time 40.0 hour
Air bomb; IEC 60811
Tensile Modulus 0.00710 GPa
@Strain 150 %
1.03 ksi
@Strain 150 %
IEC 60811
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 4.00e+15 ohm-cm>= 4.00e+15 ohm-cmIEC 60502
Dielectric Strength 39.0 kV/mm991 kV/inASTM D149
 
Processing PropertiesMetricEnglishComments
Zone 1 140 °C284 °F
Zone 2 160 °C320 °F
Zone 3 180 °C356 °F
Zone 4 190 °C374 °F
Die Temperature 205 °C401 °F
Head Temperature 190 °C374 °F
 
Descriptive Properties
Hot Set Test0Residual Value, IEC 811
 0.6250°C - 20 N/cm2, IEC 811
Insulation Constant19000 MO . KmIEC 60502

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCROS133 / 294217

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.