MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Exxtral™ HMU 208 Performance Polyolefin
Categories: Polymer; Thermoplastic; Ethylene Butyl Acrylate

Material Notes: Product Description: A specialty thermoplastic polyolefin resin, black colored, with high stiffness and release agent for automotive HVAC and under-the-hood applications.

Availability: Africa & Middle East, Asia Pacific, Europe, South America and North America

Features:

  • Good Dimensional Stability
  • Good Mold Release
  • Ultra High Stiffness
Uses:
  • Automotive Applications
  • Automotive Exterior Parts
  • Automotive Exterior Trim
  • Automotive Interior Parts
  • Automotive Under the Hood
  • Compounding
Processing Method: Injection Molding

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ISO 1183
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C
12 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 27.0 MPa3920 psiISO 527-2/50
Tensile Strength, Yield 34.0 MPa4930 psiISO 527-2/50
Elongation at Break 19 %19 %ISO 527-2/50
Elongation at Yield 4.0 %4.0 %ISO 527-2/50
Tensile Modulus 2.75 GPa399 ksiSecant; ISO 527-2
Charpy Impact Unnotched 3.57 J/cm²17.0 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.294 J/cm²
@Temperature 22.8 °C
1.40 ft-lb/in²
@Temperature 73.0 °F
Complete Break; ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C248 °FISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 63.9 °C147 °FISO 75-2/A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Exxtral™ HMU 216 Performance Polyolefin
Polyplastic Armlen® PP MF 25-3-901 Polypropylene, 20% Mineral Filled
ExxonMobil Exxtral™ HMU 405 Performance Polyolefin
ExxonMobil Exxtral™ HMU 404 Performance Polyolefin
ExxonMobil Exxtral™ HMU 301 Performance Polyolefin

PEX99376 / 175612

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.