MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Haynes HR-224® Nickel Alloy
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Alloy with excellent oxidation resistance and improved fabricability and weldability compared to HAYNES® 214® alloy. This Ni–27.5Fe–20Cr–3.8Al alloy achieves superior oxidation resistance through the formation of a tightly adherent alumina protective scale. It exhibits excellent ductility and formability characteristics, with weldability on par with nickel-iron-chromium alloys of substantially lower aluminum contents. Potential uses include heat recuperators, automotive catalytic converters and heat shields, strand annealing furnace tubulars, and other severely oxidizing environments.

Data provided by the manufacturer, Haynes International, Inc.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 481 MPa
@Temperature 760 °C
 739 MPa
@Temperature 25.0 °C
Tensile Strength, Yield 342 MPa
@Strain 0.2 %,
Temperature 25.0 °C
 401 MPa
@Strain 0.2 %,
Temperature 760 °C
Elongation at Break 27 %
@Temperature 760 °C
 45 %
@Temperature 25.0 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 3.8 %
Chromium, Cr 20 %
Iron, Fe 27.5 %
Nickel, Ni 48.7 %as balance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Rene 85 Nickel Superalloy
ATI Allvac® Rene 41® Nickel Superalloy, Heat Treatment: 1079°C (1975°F) + Age
Haynes 188 alloy, 0% cold reduction, 3.2 mm thick sheet
Haynes 188 alloy, 10% cold reduction, 3.2 mm thick sheet
Haynes 188 alloy, 20% cold reduction, 3.2 mm thick sheet

NHAY984 / 162646

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.