This is a general purpose thermoplastic elastomer based on TPV technology tailored for adhesion to nylon, and injection molding. Physical Form: Pellet. Standard Color: Translucent. Information provided by M. A. Hanna. M. A. Hanna and Geon merged to form PolyOne in 2000. |