MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Eneos NV80G NBR/PVC
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: SR NV is polymer alloy of NBR and polyvinyl chloride (abbreviated as“ PVC” below) that offers high oil and fuel oil resistance as well as excellent ozone resistance.

ENEOS has acquired the elastomer product lines from JSR Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Mooney Viscosity 65
@Temperature 100 °C
ML1+4
 74
@Temperature 100 °C
ML1+4, Compound (non-vulcanized)
 45
@Temperature 125 °C,
Time 61200 sec
Scorch Test, ML1, Compound (non-vulcanized)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 76Compound (vulcanized)
 60
@Temperature 40.0 °C,
Time 173000 sec
Fuel Oil B, Compound (non-vulcanized)
 63
@Temperature 120 °C,
Time 252000 sec
IRM903, Compound (vulcanized)
 77
@Temperature 120 °C,
Time 252000 sec
IRM901, Compound (vulcanized)
 78
@Temperature 120 °C,
Time 252000 sec
Air heat Aging, Compound (non-vulcanized)
Tensile Strength 20.9 MPaCompound (vulcanized)
 11.077 MPa
@Temperature 40.0 °C,
Time 173000 sec
Fuel Oil B, Compound (non-vulcanized)
 20.482 MPa
@Temperature 120 °C,
Time 252000 sec
IRM903, Compound (vulcanized)
 21.318 MPa
@Temperature 120 °C,
Time 252000 sec
IRM901, Compound (vulcanized)
 21.527 MPa
@Temperature 120 °C,
Time 252000 sec
Air heat Aging, Compound (non-vulcanized)
Elongation at Break 400 %Compound (vulcanized)
 228 %
@Temperature 40.0 °C,
Time 173000 sec
Fuel Oil B, Compound (non-vulcanized)
 260 %
@Temperature 120 °C,
Time 252000 sec
Air heat Aging, Compound (non-vulcanized)
 264 %
@Temperature 120 °C,
Time 252000 sec
IRM901, Compound (vulcanized)
 336 %
@Temperature 120 °C,
Time 252000 sec
IRM903, Compound (vulcanized)
100% Modulus 6.00 MPaCompound (vulcanized)
300% Modulus 18.0 MPaCompound (vulcanized)
Resilience 36[%], Rebound, Compound (vulcanized)
Tear Strength 53.0 kN/mCompound (vulcanized)
Compression Set 23 %
@Temperature 100 °C,
Time 252000 sec
Compound (vulcanized)
 30 %
@Temperature 120 °C,
Time 252000 sec
Compound (vulcanized)
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -33.0 °C
 
Descriptive Properties
Acrylonitrile ContentMedium
Delta;V100 (%)2Distilled Water 70 hr at 40°C, Compound (non-vulcanized)
 28Fuel Oil B 48 hrs at 40°C, Compound (non-vulcanized)
 -3IRM901 70 hrs at 120°C, Compound (vulcanized)
 54Fuel Oil C 48 hrs at 40°C, Compound (non-vulcanized)
 7IRM903 70 hrs at 120°C, Compound (vulcanized)
 77Fuel Oil C/Ethanol 48 hrs at 40°C, Compound (non-vulcanized)
Extrusion Test376 cc/min80°C, 25 rpm, Extrusion Volume
 464 cm/min80°C, 25 rpm, Extrusion Length
 6280°C, 25 rpm, Die Swell %
Flex Test2Growth 2 to 15 mm (Thousand Times)
 20Occurrence(Thousand Times)
Flow Rate74Q×104, 80°C, 100 kg, Kokahiki Flow tester
JSR Mold Curast Test 160°C, Minutes3tc(10)
 6tc(90)
Low-Temperature Torsion Test-26°Ct10
 -36°Ct100
Mill Contraction 50°C (%)33
NBR/PVC85/15
Ozone Degradability TestB-2Dynamic 0 to 20% Elongation, 50 ppm 5 Hours at 40°C
 NCStatic 20% Elongation, 50 ppm 5 Hours at 40°C
Product formSheet
Product StainSS

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PJSRC8079 / 295395

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.