MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Versalis Clearflex® CM 406 Hexene Copolymer Linear Low Density Polyethylene  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Hexene, Film Grade

Material Notes: Clearflex CM 406 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for cast film extrusion.

Films manufactured with Clearflex CM 406 are characterized by high clarity, optimum elongation at break and optimum impact and tear resistance.

Main Applications: Clearflex CM 406 is recommended for the production of low cling cast film with optimum optical properties and good mechanical resistance.

Information provided by Polimeri Europa.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.926 g/cc0.926 g/ccISO 1183
Thickness 8.00 - 50.0 microns0.315 - 1.97 milRecommended
Melt Flow 3.6 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.6 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 11.0 MPa1600 psiISO 527-3
Film Tensile Strength at Yield, TD 11.0 MPa1600 psiISO 527-3
Film Elongation at Break, MD 730 %730 %ISO 527-3
Film Elongation at Break, TD 850 %850 %ISO 527-3
Coefficient of Friction, Dynamic >= 0.50>= 0.50ISO 8295
Elmendorf Tear Strength, MD 8.152 g/micron207.1 g/milISO 6383-2
Elmendorf Tear Strength, TD 18.342 g/micron465.89 g/milISO 6383-2
Dart Drop Test 90.0 g0.198 lbF50; ISO 7765-1
Film Tensile Strength at Break, MD 36.0 MPa5220 psiISO 527-3
Film Tensile Strength at Break, TD 30.0 MPa4350 psiISO 527-3
1% Secant Modulus, MD 240 MPa34800 psiISO 527-3
1% Secant Modulus, TD 250 MPa36300 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 127 °C261 °FInternal method
Vicat Softening Point 103 °C
@Load 1.00 kg
217 °F
@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -70.0 °C<= -94.0 °FASTM D746
 
Optical PropertiesMetricEnglishComments
Haze 4.0 %4.0 %ISO 14782
Gloss 85 %85 %45°; ASTM D2457
Transmission, Visible 90 %90 %clear; thickness not quantified

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENG073 / 124467

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.