MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Chosun Refractories A40 Special High-Density Gunning Castable
Categories: Ceramic

Material Notes:

Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 2.18 g/cc
@Temperature 1000 °C,
Time 10800 sec
 2.18 g/cc
@Temperature 1350 °C,
Time 10800 sec
 2.21 g/cc
@Temperature 110 °C,
Time 86400 sec
Porosity 18 %
@Temperature 110 °C,
Time 86400 sec
 22 %
@Temperature 1350 °C,
Time 10800 sec
 22.5 %
@Temperature 1000 °C,
Time 10800 sec
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.008829 GPa
@Temperature 110 °C,
Time 86400 sec
 0.00981 GPa
@Temperature 1000 °C,
Time 10800 sec
 0.012753 GPa
@Temperature 1350 °C,
Time 10800 sec
 
Thermal PropertiesOriginal ValueComments
Shrinkage -0.100 %
@Temperature 1000 °C,
Time 10800 sec
 -0.0600 %
@Temperature 110 °C,
Time 86400 sec
 0.050 %
@Temperature 1350 °C,
Time 10800 sec
 
Component Elements PropertiesOriginal ValueComments
Al2O3 40 %
SiO2 45 %
 
Descriptive Properties
Main ApplicationsBlast furnace shaft
Material Required for Estimating (kg/m3)2,300

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CCHOS229 / 124173

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.