MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Covestro Pergut® S 20 Chlorinated rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Chlorinated rubber. Binder for, among other things, anticorrosion-, concrete floor coatings and road marking paints.

Properties / Applications: Pergut® S 20 can be used to formulate fast-drying anticorrosion coatings with good weather stability and resistance to water and chemicals. It can also be used in abrasion-resistant concrete floor coatings and road marking paints.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.50 g/cc1.50 g/ccDIN 53 479
Viscosity 16 - 24 cP16 - 24 cP18.5 % in toluene; DIN 53 015
Ash 0.30 %0.30 %DIN 53 568
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.30 %<= 0.30 %DIN 51 777
 
Component Elements PropertiesMetricEnglishComments
Chlorine, Cl >= 64.5 %>= 64.5 %DIN EN ISO 1158
 
Descriptive Properties
Black speck value18.5 % in toluene
Color<7Iodine color value, 18.5 % in toluene, DIN EN 1557
Content<0.005%Tetrachloromethane content, 2208-0005501-14D
 <2.5%Toluene content, 2208-0005501-14D
Turbidity18.5 % in toluene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOVEST0955 / 202738

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.