MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sandvik 22.9.3.LR Covered electrodes
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Sandvik 22.9.3.LR is a covered electrode with rutile acid coating for welding of duplex (ferritic austenitic) stainless steels of UNS S31803/S32205 type (e.g. Sandvik SAF 2205). It is characterized by very good welding properties and gives an austenitic ferritic chromium/nickel/molybdenum weld metal with an extremely low carbon content for service temperatures up to 250 C (480 F). Spray transfer gives a bead with a finely rippled surface. There is little spatter and very good slag removal. Sandvik 22.9.3.LR is particularly suited for welding in tubes.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 700 MPa102000 psi
Tensile Strength, Yield 500 MPa
@Strain 0.2 %
72500 psi
@Strain 0.2 %
Elongation at Break 20 %20 %
Charpy Impact  40.0 J
@Temperature -40.0 °C
29.5 ft-lb
@Temperature -40.0 °F
 48.0 J
@Temperature 20.0 °C
35.4 ft-lb
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 250 °C482 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.030 %<= 0.030 %
Chromium, Cr 23 %23 %
Manganese, Mn 0.80 %0.80 %
Molybdenum, Mo 3.0 %3.0 %
Nickel, Ni 9.0 %9.0 %
Nitrogen, N 0.15 %0.15 %
Phosphorus, P <= 0.030 %<= 0.030 %
Silicon, Si <= 0.90 %<= 0.90 %
Sulfur, S <= 0.025 %<= 0.025 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Outokumpu 2205 Duplex Stainless Steel
Industeel URANUS® 45N+ 22% Cr Austenitic-Ferritic Duplex Stainless Steel
Carlson 2205 (UNS S32205) Duplex Stainless Steel
Titanium Ti-6Al-4V (Grade 5), Annealed
Titanium Grade 2

NSANDV5117 / 199681

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.