MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Röhm ACRYLITE® Satinice optimum light diffusion Colorless 0D010 DF Extruded Acrylic Sheet
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Extruded

Material Notes: Available Forms: Flat Sheets
Masking: TP - Poly both sides
Properties: Light Diffusing
Optical Properties: Translucent; UV Stabilized
Surface: Fingerprint Resistant; Frosted surface
Weatherability: Indoor; Outdoor
Sizes: 48” x 96”
Thicknesses: 0.060”; 0.080”; 0.098”; 0.118”; 0.177”; 0.220”; 0.236”; 0.354”; 0.472”
Applications: Architectural and Decorative Lighting Fixtures; Artistic Design; Commercial Lighting; Displays; Distancing Applications; Dividers and Decorative Panels ; Exhibit and Tradeshows; Flat Sign Faces; Formed Sign Faces; Furniture; Glazing; Millwork; Pan Sign Faces; Retail Storefront Design; Set Design; Skylights and Daylighting; Wall Signs and Wayfinding

Information provided by Roehm America LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Optical PropertiesMetricEnglishComments
Transmission, Visible  65 %
@Thickness 12.0 mm
65 %
@Thickness 0.472 in
 68 %
@Thickness 8.99 mm
68 %
@Thickness 0.354 in
 78 %
@Thickness 5.99 mm
78 %
@Thickness 0.236 in
 80 %
@Thickness 5.59 mm
80 %
@Thickness 0.220 in
 82 %
@Thickness 4.50 mm
82 %
@Thickness 0.177 in
 86 %
@Thickness 3.00 mm
86 %
@Thickness 0.118 in
 87 %
@Thickness 2.49 mm
87 %
@Thickness 0.0980 in
 90 %
@Thickness 2.03 mm
90 %
@Thickness 0.0800 in
 91 %
@Thickness 1.52 mm
91 %
@Thickness 0.0600 in
 
Descriptive Properties
ColorColorless

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PROHM9104 / 319721

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.