MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Hostalen PP H1850 Polypropylene Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Hostalen PP H1850 is a very low flow homopolymer with good stiffness toughness balance. The grade features yellowing resistance in contact with cooling water. Typical customer use is automotive expansion tanks. Hostalen PP H1850 is not intended for medical and pharmaceutical applications. Applications: Non-fuel Reservoirs, Under hood

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccISO 1183-1
Melt Flow 1.2 g/10 min
@Load 5.00 kg,
Temperature 230 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 33.0 MPa50mm/min; ISO 527-1,-2
Elongation at Yield 14 %50mm/min; ISO 527-1,-2
Tensile Modulus 1300 MPa1% secant; ISO 527-1,-2
Charpy Impact Unnotched NBType 1, edgewise, Notch A; ISO 179
Charpy Impact, Notched 11.0 kJ/m²
@Temperature 23.0 °C
Type 1, Edgewise, Notch A; ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °Cunannealed; ISO 75B-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 52.0 °Cunannealed; ISO 75A-1,-2
Vicat Softening Point 155 °CA50; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Hostalen PP H2493 Polypropylene Copolymer
LyondellBasell Hostalen PP HP1886 Polypropylene Copolymer
A. Schulman POLYFORT™ PP 3719 Impact Copolymer Polypropylene
A. Schulman POLYFLAM™ RPP 1133 Flame Retardant, Copolymer Polypropylene
A. Schulman POLYFLAM™ RPP 1021 General Purpose Copolymer Polypropylene

PEQT8505 / 220140

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.