MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Syensqo (Solvay Specialty Polymers) Tecnoflon® TN Fluorelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer

Material Notes: TECNOFLON® TN is a high viscosity fluoroelastomer terpolymer. TN is well suited for applications requiring better chemical resistance and/or long term heat resistance compared to fluoroelastomer copolymers. It can be blended with other polymers of the Tecnoflon® family to meet specific requirements. TN does not contain curatives, therefore the proper levels of Tecnoflon® FOR M1 and Tecnoflon® FOR M2 must be added to achieve required properties. It can also be cured with diamines.

Some of the basic properties of TECNOFLON® TN are:
- Excellent chemical resistance
- Good compression set
- Excellent mold release
- Lack of mold fouling
- Superior mold flow

Tecnoflon® TN can be used for compression and transfer molding of shaft seals, valve stem seals, O-rings, gaskets, seals or any item requiring excellent chemical resistance. Tecnoflon® TN can be combined with the cure system and other typical fluoroelastomer compounding ingredients. Mixing can be accomplished with two-roll mills or internal mixers.
This material can be extruded into hoses or profiles and can be calendered to make sheet stocks or belting. Finished goods can be produced by a variety of rubber processing methods.

Applications: Belts/Belt Repair; Blending; Gaskets; Hose; Profiles; Seals; Sheet; Valves/Valve Parts

Features: Chemical Resistant; Good Flow; Good Mold Release; Heat Aging Resistant; High Viscosity; Low Compression Set; Terpolymer

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Mooney Viscosity 67
@Temperature 121 °C
67
@Temperature 250 °F
ML 1+10; ASTM D1646
 
Component Elements PropertiesMetricEnglishComments
Fluorine, F 68 %68 %
 
Descriptive Properties
AvailabilityEurope
 North America
ColorTranslucent
FormsPellets
ProcessingCalendering; Compounding
 Compression Molding; Extrusion; Resin Transfer Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4539 / 280339

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.