MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

HB Chemical Cilbond® 10E Bonding Agent
Categories: Other Engineering Material

Material Notes: Cilbond 10E bonds NBR compounds with high and low acrylonitirle contents with equal effectiveness and is the first choise for ACM compounds. Cilbond 10E is particularly suitable for HNBR and highly extended NBR, PVC/NBR blends and Vamac® G and Vamac® D, where good resistance to adhesive ingredients migrating out of the elastomer is required. It bond to all metal substrates and polar thermoplastics such as polyamides, PPO, PPS, PES and POM and thermoset plastics such as PF, MF, RF, GRP/FRP and epoxies.

Benefits; This extremely tough dry films of Cilbond 10E means that coated components can be subjected to considerable mechanical handling, without fear of chipping or peeling of the bonding agent. Cilbond 10E also resists wiping on injection molding and does not mold foul. Cilbond 10E bonds effectively at low and high temperatures (between 265°F and 390°F) and has excellent pre-baked resistance (up to 30 minutes at 320°F)

Information provided by HB Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.940 g/cc0.940 g/cc
Solids Content 23 %23 %
Volatiles 73.5 %73.5 %
Viscosity Measurement 14
@Temperature 25.6 °C
14
@Temperature 78.0 °F
[sec], No 3 Zahn Cup
 
Thermal PropertiesMetricEnglishComments
Flash Point 2.22 °C36.0 °FAbel Pensky
 
Processing PropertiesMetricEnglishComments
Shelf Life 18.0 Month18.0 Month
 
Descriptive Properties
AppearanceGrey Liquid
Bonding Temperature365-430°F
Content0.717HAP
In-Service Temperature Resistance-60-340°F
Typical Coverage405-610 ft2/US galas a On-Coat System
 610-815 ft2/US galas a Primer
VOC0.735

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHBCHEM022 / 317441

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.