MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Celanese Zytel® RS 30G30L NC010 Nylon 610
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610)

Material Notes: 30% Glass Reinforced Renewably Sourced Polyamide 610 Developed for Extrusion

Zytel RS 30G30L NC010 is a lubricated 30% glass fiber reinforced polyamide 610 resin containing a minimum of 40% renewably sourced ingredients by weight (60% based on polymer

Former DuPont product acquired by Celanese in 2022.

Key Words: PA610-GF30
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³
 1.31 g/cc0.0473 lb/in³DAM; ISO 1183
Moisture Absorption 1.20 %
@Thickness 2.00 mm
1.20 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Viscosity  93100 cP
@Shear Rate 5000 1/s,
Temperature 280 °C
93100 cP
@Shear Rate 5000 1/s,
Temperature 536 °F
ISO 11403-1 -2
 123000 cP
@Shear Rate 5000 1/s,
Temperature 260 °C
123000 cP
@Shear Rate 5000 1/s,
Temperature 500 °F
ISO 11403-1 -2
 135400 cP
@Shear Rate 5000 1/s,
Temperature 250 °C
135400 cP
@Shear Rate 5000 1/s,
Temperature 482 °F
ISO 11403-1 -2
 305600 cP
@Shear Rate 500 1/s,
Temperature 280 °C
305600 cP
@Shear Rate 500 1/s,
Temperature 536 °F
ISO 11403-1 -2
 420900 cP
@Shear Rate 500 1/s,
Temperature 260 °C
420900 cP
@Shear Rate 500 1/s,
Temperature 500 °F
ISO 11403-1 -2
 491800 cP
@Shear Rate 500 1/s,
Temperature 250 °C
491800 cP
@Shear Rate 500 1/s,
Temperature 482 °F
ISO 11403-1 -2
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inDAM; ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/inDAM; ISO 294-4 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 130 MPa18900 psi50%RH; ISO 527-1/-2
 160 MPa23200 psiDAM; ISO 527-1/-2
Elongation at Break 5.0 %5.0 %DAM; ISO 527-1/-2
 7.0 %7.0 %50%RH; ISO 527-1/-2
Tensile Modulus 6.50 GPa943 ksi50%RH; ISO 527-1/-2
 8.50 GPa1230 ksiDAM; ISO 527-1/-2
Izod Impact, Notched (ISO) 16.0 kJ/m²7.61 ft-lb/in²DAM; ISO 180/1A
 17.0 kJ/m²8.09 ft-lb/in²50%RH; ISO 180/1A
Charpy Impact Unnotched 9.50 J/cm²45.2 ft-lb/in²DAM; ISO 179/1eU
 9.50 J/cm²45.2 ft-lb/in²50%RH; ISO 179/1eU
Charpy Impact, Notched 1.65 J/cm²7.85 ft-lb/in²DAM; ISO 179/1eA
 1.65 J/cm²7.85 ft-lb/in²50%RH; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 2.28 J/g-°C0.545 BTU/lb-°F
Thermal Conductivity 0.260 W/m-K1.80 BTU-in/hr-ft²-°Fof melt
Melting Point 224 °C435 °FDAM; 10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 200 °C392 °FDAM; ISO 75-1/-2
Glass Transition Temp, Tg 50.0 °C122 °FDAM; 10°C/min; ISO 11357-1/-2
 
Descriptive Properties
AdditivesLubricants
 Release agent
Delivery formPellets
Part Marking Code>PA610-GF30<ISO 11469
ProcessingInjection Molding
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
Resin IdentificationPA610-GF30ISO 1043
Special characteristicsLight stabilized or stable to light

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Zytel® 77G33HS1L NC010 Nylon 612
Celanese Elvamide® 8061 PA6/66/610
DuPont Mobility and Materials Zytel® RS 30G30HSL BK038A Nylon 610
Akro-Plastic Akromid® S3 GF15 1 (3223) PA 6.10 Dry, 15% Glass Filled
DuPont Mobility and Materials Zytel® PLUS PLS95G35DH1 BK031 Nylon

PZDSY5475 / 161302

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.