MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Encom Polymers QuadPoly CP2540 Polypropylene, Super High Impact QuadPolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Appearance: Black, Natural or Colors

Processing Methods: Injection, Profile Extrusion, Thermoforming, Molding

Applications: Automotive, FDA, Business Equip., Material Handling, Lawn & Garden

Information provided by EnCom Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Maximum Moisture Content 0.0200.020
Melt Flow 2.1 g/10 min
@Load 2.16 kg,
Temperature 230 °C
2.1 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9797ASTM D785
Tensile Strength, Yield 33.0 MPa4790 psiASTM D638
Elongation at Break 25 %25 %ASTM D638
Flexural Modulus 1.828 GPa265.1 ksiASTM D790
Izod Impact, Notched NBNBASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 118 °C244 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 188 - 216 °C370 - 420 °F
Middle Barrel Temperature 199 - 232 °C390 - 450 °F
Front Barrel Temperature 199 - 232 °C390 - 450 °F
Nozzle Temperature 193 - 227 °C380 - 440 °F
Melt Temperature 204 - 260 °C400 - 500 °F
Mold Temperature 18.3 - 54.4 °C65.0 - 130 °F
Drying Temperature 93.3 °C200 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENCOM202 / 266216

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.