Martinal® OL-104 GO aluminum hydroxide is fine precipitated with a proprietary coating. It is designed for improved elongation at break, rheological and electrical properties especially in thermoplastic or crosslinked EVA/PE or rubber compounds.Information provided by J.M. Huber Corporation |