MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Haysite H208 Polyester, Magnetic Permeable
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: Grade H208 has high magnetic permeability and excellent retention of properties after heat aging at elevated temperatures. This unique combination of properties allows Grade H208 to be used in various motor, transformer, coil, and other applications requiring low hysteresis or magnetic flux losses.

Information provided by Haysite

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 3.28 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 35 - 40ASTM D2583
Flexural Strength 16300 psiLW; ASTM D790
 17920 psiCW; ASTM D790
Flexural Modulus 877800 psiLW; ASTM D790
 974100 psiCW; ASTM D790
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+6 ohm-cmASTM D257
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.2 µin/in-°FASTM D696-08
Specific Heat Capacity 0.6434 J/g-°CASTM E-1269-05
Thermal Conductivity 0.717 W/m-KASTM E-1925-06
Maximum Service Temperature, Inert 155 °CIEEE

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CRP Technology Windform® XT 2.0 Polyamide-Carbon Fiber Composite
Norplex-Micarta SP525M (WaveMax 5000) Glass Fabric
Overview of materials for Epoxy Cure Resin
Overview of materials for Epoxy Adhesive
IDI Composites Rosite® C100CB ESD BMC, Conductive Thermoset Polyester, 15% Glass Reinforced

PHAY506 / 142462

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.