MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Akrochem Antioxidant 1010
Categories: Other Engineering Material

Material Notes: Product Description: Antioxidant 1010 is a non-staining, high molecular weight, hindered phenolic antioxidant. Because of its low volatility, Antioxidant 1010 imparts excellent heat stability and color retention, with good compatibility and low extractability. Outstanding for use with peroxide cures due to minimal cure interference.

Application: Antioxidant 1010 finds application in plastics, rubber, latex, varnishes, adhesives, TPR's and Hot Melts. In plastics, antioxidant 1010 provides excellent antioxidant performance in Polyethylene, Polystyrene, Polyacetal, PVC, AS resin, Methacrylic resin, Polycarbonate, Polyester, and Polymethylpentene as well as many others. In rubbers, Antioxidant 1010 can be used in SBR, EPR, EPDM, Polybutadiene, Neoprene, Nitrile, Polyisoprene, and many other synthetic rubbers. Typical dosage is 0.02% - 0.50% by weight. FDA regulations with Antiox 1010 clearance include 175.105 and 178.2010 [if used according to these regulations, then 177.2600 (Rubber articles) will allow 1010 usage].

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/cc
Volatiles <= 0.30 %
Ash <= 0.10 %
 
Thermal PropertiesOriginal ValueComments
Melting Point 110 - 125 °C
 
Descriptive Properties
Appearancewhite powder
Assay>98%
Color>97%Color of Solution at 425 nm
 >98%Color of Solution at 500 nm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH489 / 315407

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.