MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Special Metals INCOLOY® Alloy 330
Categories: Metal; Superalloy; Iron Base

Material Notes: A nickel-iron-chromium alloy with an addition of silicon for enhanced oxidation resistance. It has good strength at high temperatures and excellent resistance to carburizing and oxidizing atmospheres. The alloy's austenitic microstructure remains stable during long-time exposure to high temperature. Used in industrial heating for furnace muffles, retorts, and conveyor systems and for heat-treating baskets and fixtures. Standard product forms are round, flats, forging stock, plate, sheet, strip, and wire.

Data provided by the manufacturer, Special Metals.

Key Words: SAE AMS 5592, 5716; SAE J405, J412, UNS N08330; ASTM B 511, B 512, B 535, B 536, B 546, B 710; ASME SB-511, SB-536, SB-710, Boiler Code Sections I, VIII, IX
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.08 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 600 MPaAnnealed prior to test
 480 MPa
@Temperature 550 °C
Annealed prior to test
Tensile Strength, Yield 280 MPa
@Strain 0.2 %
Annealed prior to test
 170 MPa
@Strain 0.2 %,
Temperature 550 °C
Annealed prior to test
Elongation at Break 45 %Annealed prior to test.
 45 %
@Temperature 550 °C
Annealed prior to test.
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0001017 ohm-cm
Magnetic Permeability 1.02at 200 Oersted (15.9 kA/m)
 
Thermal PropertiesOriginal ValueComments
CTE, linear 14.9 µm/m-°C
@Temperature 20.0 - 100 °C
Specific Heat Capacity 0.460 J/g-°C
Thermal Conductivity 12.4 W/m-K
Melting Point 1345 - 1425 °C
Solidus 1345 °C
Liquidus 1425 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.080 %
Chromium, Cr 17 - 20 %
Iron, Fe 43 %As remainder
Manganese, Mn <= 2.0 %
Nickel, Ni 34 - 37 %
Phosphorus, P 0.030 %
Silicon, Si 0.75 - 1.5 %
Sulfur, S <= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Special Metals INCOLOY® Alloy 800HT™
Special Metals INCOLOY® Alloy 800
Special Metals INCOLOY® Alloy 925
Special Metals INCOLOY® Alloy 825
Special Metals NILO® 365 Controlled-Expansion Alloy

NIND00 / 17517

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.