MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Envalior Arnite® TV4 461 (PBT+PET)-GF30
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); PBT + PET Blend, Glass Filled

Material Notes: 30% Glass Reinforced

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.55 g/ccISO 1183
Water Absorption 0.30 %Sim. To ISO 62
Moisture Absorption 0.150 %Sim. To ISO 62
Viscosity 12500 cP
@Shear Rate 100000 1/s,
Temperature 270 °C
 16000 cP
@Shear Rate 100000 1/s,
Temperature 250 °C
 20000 cP
@Shear Rate 100000 1/s,
Temperature 230 °C
 600000 cP
@Shear Rate 1 1/s,
Temperature 270 °C
 800000 cP
@Shear Rate 1 1/s,
Temperature 250 °C
 1.75e+6 cP
@Shear Rate 1 1/s,
Temperature 230 °C
Linear Mold Shrinkage, Flow 0.011 cm/cmSim. To ISO 294-4
Linear Mold Shrinkage, Transverse 0.0032 cm/cmSim. To ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 130 MPaISO 527-1/-2
Elongation at Break 2.4 %ISO 527-1/-2
Tensile Modulus 9.90 GPaISO 527-1/-2
Charpy Impact Unnotched 45.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
 45.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 9.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 9.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Dielectric Constant 3.9
@Frequency 1e+6 Hz
IEC 60250
 4.1
@Frequency 100 Hz
IEC 60250
Dissipation Factor 0.0015
@Frequency 100 Hz
IEC 60250
 0.016
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 275 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 40.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 60.0 µm/m-°CISO 11359-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 225 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 205 °CISO 75-1/-2
Flammability, UL94 HB
@Thickness 1.60 mm
IEC 60695-11-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultradur® B 4040 G6 30% Glass Filled PBT + PET
E-Polymers TEKALOY® F50G30 30% Glass Fiber Reinforced PBT/PET Alloy
Envalior Arnite® TV4 461 KL (PBT+PET)-GF30
LG Chemical Lupox® SG5300 PBT+PET+GF30%
Eurotec® Tecodur® PB70 GR35 NL100 HS01 PBT/PET, 35% glass fiber reinforced, heat stabilized, natural

PDSM9769 / 161390

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.