MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Wingate Alloys Winco Mang 11-14% Manganese, Work Hardening Steel
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: A non-magnetic alloy steel that work hardens under severe impact conditions.
    Advantages:
  • Provides longer life in shot blast cabinet operations. Winco Mang’s resiliency will prolong use of steel shot and result in greater efficiency.
  • Can be torch cut, welded with a high tensile electrode-a stainless steel rod, AWS E308-16 or E310-15, is recommended. A high manganese rod (11-14)% can also be used with satisfactory results.
  • Winco Mang can be formed cold for most applications.
Applications: Shot blast equipment, guide rails, pangborn liners, chute liners, wheelabrator parts, hoppers, foundry shakeout machines, crusher liners, bucked teeth and crusher hammers.

Information from Wingate Alloys Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 180 - 200
 550 - 600work hardened
Tensile Strength 155000 psi
Elongation at Break 75 %2[in]
Reduction of Area 55 %
 
Component Elements PropertiesOriginal ValueComments
Manganese, Mn 11 - 14 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Industeel CREUSABRO® M Wear Resistant Steel
AISI Type S24000 Stainless Steel, plate
205 Austenitic Stainless Steel (UNS S20500)
Tenelon Austenitic Stainless Steel, UNS S21400 (Composition Spec)
MetalTek Nitronic® 33 Austenitic Stainless Steel

NWINGA06 / 122070

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.