MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
ChenGuang PVdF RESIN
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF)

Material Notes: Molecular formula: [CH2--CF2]n

Properties: PVdF namely Polyvinylidene fluoride is a kind of crystal polymer with low melting point (160 ~ 170), high mechanical properties, good resistance to wear , to high temperature, to corrosion, to weather and as well with good electric insulation, high dielectric constant. Also it is anti-ultraviolet ray, anti-radiation and easily machined. With low processing temperature and good melting flow, it could be processed easily to make pipe, plate, rod, film and fiber. Its heat conductivity is poor.

Usage: Used as good anti-corrosion material in chemical industry, especially in the circumstances of acid, organic solvents, halogens, as well as their mixture. Widely used as insulation material in electronic / electric industries, computer industry, air/space industry to make cable sheathing, coating layer, and condenser film, etc.

Information provided by ChenGuang Research Institute of Chemical Industry

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.73 - 1.79 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break >= 39.0 MPa
Elongation at Break >= 100 %
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.00e+11 ohm-cm
Dielectric Constant >= 6.0
@Frequency 1e+6 Hz
Dissipation Factor >= 0.80
@Frequency 1e+6 Hz

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHENGU037 / 255636

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.