MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Nucrel® 30705 Ethylene Acrylic Acid
Categories: Polymer; Thermoplastic; Ethylene Acrylic Acid

Material Notes: Nucrel® 30705 is an ethylene-acrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to process polyethylene resin. This resin may also be used in conventional blown and cast film extrusion and coextrusion equipment.

Uses:

  • Adhesives
  • Packaging
  • Sealants

Composition: 7 % By Weight Acrylic Acid comonomer content

Nucrel® 30705 conforms to the U.S. Code of Federal Regulations, Title 21, Paragraph 177.1310, covering its use as a food contact surface subject to the extractives limitations on the finished food contact article as described in the regulation.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 g/ccASTM D792, ISO 1183
Melt Flow 5.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238, ISO 1133
 
Thermal PropertiesOriginal ValueComments
Melting Point 89.0 °CFreezing Point; ASTM D3418, ISO 3146
 107 °CASTM D3418, ISO 3146
Vicat Softening Point 85.0 °CASTM D1525, ISO 306
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 310 °C
Feed Temperature 135 °CBlown Film Coextrusion
 185 °CExtrusion Coating
Zone 2 160 °CBlown Film Coextrusion
 235 °CExtrusion Coating
Zone 3 185 °CBlown Film Coextrusion
 285 °CExtrusion Coating
Zone 4 185 °CBlown Film Coextrusion
 300 °CExtrusion Coating
Zone 5 185 °CBlown Film Coextrusion
 300 °CExtrusion Coating
Adapter Temperature 185 °CBlown Film Coextrusion
 300 °CExtrusion Coating
Die Temperature 185 °CBlown Film Coextrusion
 300 °CExtrusion Coating
Melt Temperature 160 - 285 °CExtrusion Coating

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Nucrel® 3990L Ethylene Acrylic Acid
Dow Nucrel® 30907 Ethylene Acid Copolymer Resin
Dow Nucrel® 31001 Ethylene-Acrylic Acid Copolymer Resin for Blown and Cast Film
Arkema LOTADER® 8200 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
Dow Nucrel® 3990 Ethylene-Acrylic Acid Copolymer Resin for Extrusion Coating/Laminating

PDTA4970 / 170410

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.