MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Kennametal Stellite Tribaloy® T-400 Cobalt Alloy
Categories: Metal; Nonferrous Metal; Cobalt Alloy; Superalloy

Material Notes: Kennametal Stellite's™ cobalt base alloys are available as cobalt rods, cobalt electrodes, cobalt wire and cobalt powder.

The Tribaloy family of cobalt alloys feature a hard inter-metallic Laves phase, dispersed in a tough matrix of eutectic or solid solution. They exhibit outstanding resistance to high temperature wear, galling and corrosion and are particularly suitable for use where lubrication is a problem.

Information provided by Kennametal Stellite™

Key Words: UNS R30400
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 51 - 57
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.080 %
Chromium, Cr 8.5 %
Cobalt, Co >= 55.62 %as balance
Iron, Fe <= 1.5 %
Molybdenum, Mo 29 %
Nickel, Ni <= 1.5 %
Other <= 1.0 %
Silicon, Si 2.8 %
 
Descriptive Properties
Application TechniqueHVOF & thermal spray
 PTA & laser deposition

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kennametal Stellite Tribaloy® T-800
Kennametal Stellite Tribaloy® T-400C Cobalt Alloy
Kennametal Stellite Tribaloy® T-700 Nickel Alloy
Kennametal Stellite Tribaloy® 745
Kennametal Stellite Tribaloy® T-401 Cobalt Alloy

NSTA4924 / 159856

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.