MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Evonik VESTASOL® TMC-one Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: A wonderful synthesis VESTASOLR TMC -one is a raw material for a number of chemical syntheses for products used in the plastic and cosmetic industries. Brilliant finish Surface defects are greatly reduced with VESTASOLR TMC -one. It is a solvent that improves the leveling properties and gloss of coating.

Applications:

  • Coatings
  • Raw material for chemical syntheses
  • Plastics (e.g., polycarbonate)
Properties:
  • Improves leveling
  • Increases gloss
  • Improves surfaces
  • Universal solvency

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.880 g/cc0.0318 lb/in³DIN 51 757
Viscosity 2.5 cP2.5 cP
Molecular Weight 140 g/mol140 g/mol
Vapor Pressure 0.00800 bar
@Temperature 50.0 °C
6.00 torr
@Temperature 122 °F
 
Chemical PropertiesMetricEnglishComments
Total Acid Number <= 0.10<= 0.10mg KOH/mg
 
Thermal PropertiesMetricEnglishComments
Melting Point -10.0 °C14.0 °F
Boiling Point 189 °C
@Pressure 0.1013 MPa
372 °F
@Pressure 14.69 psi
DIN 53 171
Flash Point 64.0 °C147 °FDIN EN ISO 2719
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4451.445n20; DIN 51 423
 
Descriptive Properties
AppearanceClear
Color<15Hazen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIL363 / 196567

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.