MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lubrizol Pearlstick™ 5714 Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Type: Pearlstick™ 5714 TPU is a Polyether-Type Thermoplastic Polyurethane (TPU).

Features: Low Temperature Flexibility, Excellent Abrasion, Fungal, and Chemical Resistance and Hydrolytic Stability. Adhesives can be applied from solution or extruded as a melt coating. The resin is lightly dusted with calcium stearate and contains UV stabilizer.

Uses: Various adhesive and fabric coating, magnetic media binder and cast films for lamination.

Information provided by The 159 Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.11 g/ccASTM D792
Viscosity 72000 cP
@Temperature 204 °C
Melt; ASTM D-1084-88
Brookfield Viscosity 900 cP15% T.S. in THF, RVT Spindle #2, 20 RPM, 23°C
 3700 cP15% T.S. in Cyclohexanone, RVT Spindle #2, 20 RPM, 23°C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80ASTM D2240
Tensile Strength 31.0 MPaASTM D-412/D-638
Elongation at Break 530 %ASTM D-412/D-638
100% Modulus 4.80 MPa
@Strain 100 %
ASTM D-412/D-638
300% Modulus 9.00 MPa
@Strain 300 %
ASTM D-412/D-638
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 71.0 °CASTM D-1525
Ring & Ball Softening Point 174 °CASTM E-28-92
 
Descriptive Properties
Gradient Bar Tack Temperature127°C
Open Time<5 secASTM D-4497-94

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Geniosil® XL 32 Silane
Parson Adhesives PARTITE® 7440 Methacrylate Structural Adhesive
Lord Adhesives 7433 Urethane Adhesive System
ITW Plexus Plexus™ MA550 Methacrylate Adhesive
Henkel Loctite® 3102 Acrylic Light Cure Adhesive

PLUBR5012 / 238882

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.