MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC LNP™ THERMOCOMP™ Compound DX06408 Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP THERMOCOMP DX06408 compound is based on Polycarbonate (PC) resin containing 10% glass fiber. Added features of this grade include: Easy Molding, Mold Release.

Features: High Stiffness,Good Mold Release,Easy Molding,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.27 g/cc0.0459 lb/in³ISO 1183
 1.275 g/cc0.04606 lb/in³ASTM D792
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.150 %0.150 %23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/in24hrs; ASTM D955
 0.0043 cm/cm0.0043 in/in24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.0050 cm/cm0.0050 in/in24hrs; ASTM D955
 0.0051 cm/cm0.0051 in/in24hrs; ISO 294
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 83.0 MPa12000 psiASTM D638
 84.0 MPa12200 psiISO 527
Elongation at Break 3.6 %3.6 %ISO 527
 3.8 %3.8 %ASTM D638
Tensile Modulus 4.10 GPa595 ksi1 mm/min; ISO 527
 4.17 GPa605 ksi50 mm/min; ASTM D638
Flexural Strength 117 MPa17000 psiISO 178
 149 MPa21600 psiASTM D790
Flexural Modulus 3.92 GPa569 ksiISO 178
 4.28 GPa621 ksiASTM D790
Izod Impact Notched 97.0 J71.5 ft-lbASTM D256
Izod Impact, Unnotched 9.29 J/cm17.4 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 8.00 kJ/m²3.81 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 61.0 kJ/m²29.0 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 13.0 J9.59 ft-lbpeak; ASTM D3763
Impact Test 9.00 J6.64 ft-lbMultiaxial Impact; ISO 6603
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  38.1 µm/m-°C
@Temperature -40.0 - 40.0 °C
21.2 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 38.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
21.2 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  53.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
29.7 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 53.5 µm/m-°C
@Temperature -40.0 - 40.0 °C
29.7 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 141 °C286 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 141 °C
@Thickness 3.20 mm
286 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 137 °C279 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 136 °C
@Thickness 3.20 mm
277 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Zone 2 310 - 320 °C590 - 608 °F
Zone 3 320 - 330 °C608 - 626 °F
Melt Temperature 305 - 325 °C581 - 617 °FInjection Molding
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81547 / 289494

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.