MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

BASF Lupragen® N 700 1,8-Diazabicyclo-5,4,0-undecene-7
Categories: Fluid

Material Notes: Formula: C7H18N2O

CAS: 6674-22-2

Description: Lupragen® N 700 –1,8-Diazabicyclo-5,4,0-undecene-7 is a colorless to yellowish liquid, with an amine-like odor. It is miscible with water in all proportions.

Synonyms: DBU, 2,3,4,6,7,8,9,10-Octahydropyrimido[1,2-a]azepine

Applications: Intermediate used in the production of Polyurethane catalyst, Initial product for chemical syntheses and Acid binder

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.019 g/cc0.03681 lb/in³
Viscosity 26 cP26 cP
 
Thermal PropertiesMetricEnglishComments
Melting Point -70.0 °C-94.0 °F
Boiling Point 261 °C502 °F
Flash Point 116 °C241 °F
Ignition Temperature 260 °C500 °F
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 0.50 %<= 0.50 %DIN 51 777
 
Descriptive Properties
Assay98%
Total Amines0.98(N4)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Lupragen® N 100 DMCHA Dimethylcyclohexylamine
BASF Lupragen® N 107 Dimethylaminoethoxyethanol
BASF Lupragen® N 201 TEDA in DPG
BASF Lupragen® N 105 N-Methylmorpholine
BASF Lupragen® N 400 Trimethylamineoethylethanolamine

PBASG0870 / 132503

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.