MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Outokumpu 4021 Martensitic Stainless Steel
Categories: Metal; Ferrous Metal; Martensitic; Stainless Steel

Material Notes: Moderate corrosion resistant stainless steel hardenable up to 1000N/mm2. Re-sulphurized steel improves machining properties.

Applications:

  • Shafts
  • Knives
  • Fasteners
  • Surgical applications
  • Domestic applications

Available in hot rolled strip/sheet (CPP), cold rolled narrow strip, bar, and rod forms.

Key Words: EN 1.4021; ASTM 420; JIS SUS 420J1
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.70 g/ccRT
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 650 MPaOutokumpu Typical, Annealed Hot Rolled Plate (Quarto); EN 10002-1
Tensile Strength, Yield 450 MPa
@Strain 0.2 %
EN min., RT; EN 10002-1
 500 MPa
@Strain 0.2 %
Outokumpu Typical, Annealed Hot Rolled Plate (Quarto); EN 10002-1
 580 MPa
@Strain 1 %
Outokumpu Typical, Annealed Hot Rolled Plate (Quarto); EN 10002-1
 365 MPa
@Strain 0.2 %,
Temperature 400 °C
EN min.; EN 10002-5
 400 MPa
@Strain 0.2 %,
Temperature 200 °C
EN min.; EN 10002-5
 420 MPa
@Strain 0.2 %,
Temperature 100 °C
EN min.; EN 10002-5
Elongation at Break 20 %Outokumpu Typical, Annealed Hot Rolled Plate (Quarto); EN 10002-1
Modulus of Elasticity 215 GPaRT
 190 GPa
@Temperature 400 °C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000550 ohm-cmRT
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.5 µm/m-°C
@Temperature 100 °C
 12.0 µm/m-°C
@Temperature 400 °C
Specific Heat Capacity 0.460 J/g-°CRT
Thermal Conductivity 30.0 W/m-KRT
 25.0 W/m-K
@Temperature 400 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.20 %
Chromium, Cr 13 %
Iron, Fe 86.8 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Outokumpu 4028 Martensitic Stainless Steel
420 Stainless Steel
Sandvik 12C27 Strip Steel
AK Steel 420 Martensitic Stainless steel
420 Stainless Steel, annealed bar

NOUTOK01 / 18716

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.