MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

BYK Optiflo® H7500 VF Polymer
Categories: Polymer

Material Notes: Description: Optiflo H7500-VF is an aqueous solution of a hydrophobically modified nonionic polymer commonly called an associative thickener. Optiflo H7500-VF is VOC-free and APEO free.

Application: Optiflo H7500-VF is designed to thicken dispersion (latex) paints, with specific efficiencies in VAE based binder systems. It may also be used with acrylic, styrene/acrylic, and vinyl acetate copolymer latexes.

Information provided by Southern Clay Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³
Volatiles 60 %60 %
pH 7.0 - 107.0 - 10
Viscosity 2000 - 7000 cP2000 - 7000 cP
 
Descriptive Properties
Active0.175
Color/FormHazy solution

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BYK Optiflo® H3300 VF Polymer
BYK Optiflo® H3300 Polymer
BYK Opibent® MF Silicate
BYK Opibent® 987 Layered Silicate
BYK Opibent® 940 Layered Silicate

PBYK094 / 185091

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.