MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

NuSil DDU-4340 Unrestricted Drug Delivery Silicone
Categories: Polymer; Thermoset; Silicone

Material Notes: Comments: Low Consistency Elastomer

Cure System: Tin-Alkoxy

Information provided by NuSil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc1.14 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5050
Tensile Strength at Break 3.80 MPa551 psi
Elongation at Break 175 %175 %
 
Processing PropertiesMetricEnglishComments
Cure Time 30.0 min0.500 hour
Working Life 9.00 min9.00 min
 
Descriptive Properties
ColorGray to Tan

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sandvik Osprey 4340 Low Alloy Steel Powder (Grade 90% - 16)
AISI 4340 Steel, normalized, 25 mm round
AISI 4340 Steel, oil quenched 800°C (1470°F), 540°C (1000°F) temper, 100 mm (4 in.) round
430 Stainless Steel annealed sheet
AISI 4340 Steel, oil quenched 800°C (1470°F), 540°C (1000°F) temper, 25 mm round

PNUSIL471 / 142195

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.