MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Evonik VESTAKEEP® Care M40 3DF PEEK for 3D printing
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: VESTAKEEP® Care M40 3DF is extruded from naturally colored, high viscosity VESTAKEEP® Care M40 G PEEK resin. The material is designed for 3d printing of medical devices with up to 30 days body contact.
Dry properties listed below
Industrial Sector: Medical Devices , 3D Printing
Processing: 3D Printing
Delivery form: (Mono)filament
Optics: Opaque
Resistance to: Heat (thermal stability), Hydrolysis / hot water, Wear / abrasion
Conformity: Biocompatibility, Medical application
Additives: Unfilled
Applications: Monofilament
Processing: Fused deposition molding, Additive manufacturing
Special Characteristics: Semi-crystalline, High viscosity, Sterilizable
Features: Resistance to steam
Regulatory: US Pharmacopeia Class VI conformity
Color: Natural color
Chemical Resistance: Acid resistance, Alkali resistance, Solvent resistance, Grease resistance, Hydrolytically stable, Oil resistance, Oxidation resistance, General chemical resistance

Information provided by Evonik.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³ISO 1183
Water Absorption 0.400 %0.400 %Sim to ISO 62
Filament Diameter 1750 µm1750 µm
Melt Flow 11.0 g/10 min
@Load 5.00 kg,
Temperature 380 °C
11.0 g/10 min
@Load 11.0 lb,
Temperature 716 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 94.0 MPa13600 psiISO 527
Tensile Strength, Yield 94.0 MPa13600 psiISO 527
Elongation at Yield 5.00 %5.00 %ISO 527
Tensile Modulus 3.50 GPa508 ksiISO 527
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
Type of failure: C; ISO 179/1eA
 0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
Type of failure: C; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 60.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
33.3 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1/-2
Melting Point 335 °C635 °FISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 205 °C401 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 155 °C311 °FISO 75-1/-2
Vicat Softening Point  305 °C
@Load 5.10 kg
581 °F
@Load 11.2 lb
50 K/h; ISO 306
 335 °C
@Load 1.02 kg
635 °F
@Load 2.25 lb
50 K/h; ISO 306
Glass Transition Temp, Tg 152 °C306 °FISO 11357-1/-2
Flammability, UL94 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
IEC 60695-11-10
 
Descriptive Properties
ColorNatural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK7844 / 324976

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.