MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Parson Adhesives PARFIX® 3416 Cyanoacrylate Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: PARFIX 3416 is a high viscosity, cyanoacrylate adhesive with slower cure speed compare to other cyanoacrylate adhesives. This adhesive develops strong bonds on wide variety of metals, plastics, and elastomeric compounds.

Applications:

  • Specially formulated to bond various plastics, metals and elastomers.
  • Rough or irregular surfaces.
  • Applications requiring alignment time of up to 15 seconds.

Information provided by Parson Adhesives, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brookfield Viscosity 1500 cP1500 cPLVF, Spindle 1-60 rpm
 
Mechanical PropertiesMetricEnglishComments
Shear Strength 5.00 - 10.0 MPa725 - 1450 psiPolycarbonate; ASTM D1002
 6.00 - 9.03 MPa870 - 1310 psiPVC; ASTM D1002
 8.00 - 14.0 MPa1160 - 2030 psiABS; ASTM D1002
 10.0 - 15.0 MPa1450 - 2180 psiNeoprene Rubber; ASTM D1002
 10.0 - 15.0 MPa1450 - 2180 psiAcrylic; ASTM D1002
 15.0 - 22.0 MPa2180 - 3190 psi
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 24.6 kV/mm625 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 µm/m-°C50.0 µin/in-°FASTM D696
Thermal Conductivity 0.100 W/m-K0.694 BTU-in/hr-ft²-°FASTM C177
Melting Point 160 - 170 °C320 - 338 °F
Maximum Service Temperature, Air 80.0 °C176 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
Glass Transition Temp, Tg 125 °C257 °FASTM E228
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min24.0 hourFull
 
Descriptive Properties
AppearanceColorless liquid
Bonding Times<5 secNeoprene
 10-15 secPhenolics
 10-20 secAluminum
 10-30 secABS
 10-30 secPVC
 15-50 secPolycarbonate
 25-35 secSteel
 5-7 secNitrile Rubber
CompositionEthyl Cyanoacrylate Adhesive
Gap Filling0.45 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPARSN125 / 186568

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.