MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Water, H2O
Categories: Fluid

Material Notes:

Key Words: H2O
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  0.95838 g/cc
@Temperature 100 °C
0.034624 lb/in³
@Temperature 212 °F
 0.99823 g/cc
@Temperature 20.0 °C
0.036063 lb/in³
@Temperature 68.0 °F
 0.99987 g/cc
@Temperature 0.000 °C
0.036123 lb/in³
@Temperature 32.0 °F
 1.00000 g/cc
@Temperature 3.98 °C
0.0361273 lb/in³
@Temperature 39.2 °F
density = 1.00000 g/cc at 3.98°C (most dense temperature)
pH 7.07.0
Viscosity  0.2818 cP
@Pressure 0.100 MPa,
Temperature 100 °C
0.2818 cP
@Pressure 14.5 psi,
Temperature 212 °F
 0.3145 cP
@Pressure 0.100 MPa,
Temperature 90.0 °C
0.3145 cP
@Pressure 14.5 psi,
Temperature 194 °F
 0.3544 cP
@Pressure 0.100 MPa,
Temperature 80.0 °C
0.3544 cP
@Pressure 14.5 psi,
Temperature 176 °F
 0.404 cP
@Pressure 0.100 MPa,
Temperature 70.0 °C
0.404 cP
@Pressure 14.5 psi,
Temperature 158 °F
 0.4665 cP
@Pressure 0.100 MPa,
Temperature 60.0 °C
0.4665 cP
@Pressure 14.5 psi,
Temperature 140 °F
 0.547 cP
@Pressure 0.100 MPa,
Temperature 50.0 °C
0.547 cP
@Pressure 14.5 psi,
Temperature 122 °F
 0.6532 cP
@Pressure 0.100 MPa,
Temperature 40.0 °C
0.6532 cP
@Pressure 14.5 psi,
Temperature 104 °F
 0.7977 cP
@Pressure 0.100 MPa,
Temperature 30.0 °C
0.7977 cP
@Pressure 14.5 psi,
Temperature 86.0 °F
 1.002 cP
@Pressure 0.100 MPa,
Temperature 20.0 °C
1.002 cP
@Pressure 14.5 psi,
Temperature 68.0 °F
 1.307 cP
@Pressure 0.100 MPa,
Temperature 10.0 °C
1.307 cP
@Pressure 14.5 psi,
Temperature 50.0 °F
 1.793 cP
@Pressure 0.100 MPa,
Temperature 0.000 °C
1.793 cP
@Pressure 14.5 psi,
Temperature 32.0 °F
Molecular Weight 18.015 g/mol18.015 g/mol
Vapor Pressure  0.006113 bar
@Temperature 0.000 °C
4.585 torr
@Temperature 32.0 °F
 0.012281 bar
@Temperature 10.0 °C
9.2115 torr
@Temperature 50.0 °F
 0.023133 bar
@Temperature 20.0 °C
17.351 torr
@Temperature 68.0 °F
 0.023388 bar
@Temperature 20.0 °C
17.542 torr
@Temperature 68.0 °F
 0.042455 bar
@Temperature 30.0 °C
31.844 torr
@Temperature 86.0 °F
 0.073814 bar
@Temperature 40.0 °C
55.365 torr
@Temperature 104 °F
 0.12344 bar
@Temperature 50.0 °C
92.588 torr
@Temperature 122 °F
 0.19932 bar
@Temperature 60.0 °C
149.50 torr
@Temperature 140 °F
 0.31176 bar
@Temperature 70.0 °C
233.84 torr
@Temperature 158 °F
 0.47373 bar
@Temperature 80.0 °C
355.33 torr
@Temperature 176 °F
 0.70117 bar
@Temperature 90.0 °C
525.92 torr
@Temperature 194 °F
 1.01325 bar
@Temperature 100 °C
760.000 torr
@Temperature 212 °F
Surface Tension  58.91 dynes/cm
@Pressure 0.100 MPa,
Temperature 100 °C
58.91 dynes/cm
@Pressure 14.5 psi,
Temperature 212 °F
 60.82 dynes/cm
@Pressure 0.100 MPa,
Temperature 90.0 °C
60.82 dynes/cm
@Pressure 14.5 psi,
Temperature 194 °F
 62.67 dynes/cm
@Pressure 0.100 MPa,
Temperature 80.0 °C
62.67 dynes/cm
@Pressure 14.5 psi,
Temperature 176 °F
 64.47 dynes/cm
@Pressure 0.100 MPa,
Temperature 70.0 °C
64.47 dynes/cm
@Pressure 14.5 psi,
Temperature 158 °F
 66.24 dynes/cm
@Pressure 0.100 MPa,
Temperature 60.0 °C
66.24 dynes/cm
@Pressure 14.5 psi,
Temperature 140 °F
 67.94 dynes/cm
@Pressure 0.100 MPa,
Temperature 50.0 °C
67.94 dynes/cm
@Pressure 14.5 psi,
Temperature 122 °F
 69.6 dynes/cm
@Pressure 0.100 MPa,
Temperature 40.0 °C
69.6 dynes/cm
@Pressure 14.5 psi,
Temperature 104 °F
 71.2 dynes/cm
@Pressure 0.100 MPa,
Temperature 30.0 °C
71.2 dynes/cm
@Pressure 14.5 psi,
Temperature 86.0 °F
 72.75 dynes/cm
@Pressure 0.100 MPa,
Temperature 20.0 °C
72.75 dynes/cm
@Pressure 14.5 psi,
Temperature 68.0 °F
 74.23 dynes/cm
@Pressure 0.100 MPa,
Temperature 10.0 °C
74.23 dynes/cm
@Pressure 14.5 psi,
Temperature 50.0 °F
 75.64 dynes/cm
@Pressure 0.100 MPa,
Temperature 0.000 °C
75.64 dynes/cm
@Pressure 14.5 psi,
Temperature 32.0 °F
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 220.5 bar165400 torr
Critical Temperature 374.1 °C705.4 °F
Critical Density 0.322 g/cc0.0116 lb/in³
Critical Molar Volume 56.0 cm³/mol3.42 in³/mol
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.818e+7 ohm-cm1.818e+7 ohm-cm
Dielectric Constant  55.51
@Pressure 0.100 MPa,
Temperature 100 °C
55.51
@Pressure 14.5 psi,
Temperature 212 °F
 58.12
@Pressure 0.100 MPa,
Temperature 90.0 °C
58.12
@Pressure 14.5 psi,
Temperature 194 °F
 60.86
@Pressure 0.100 MPa,
Temperature 80.0 °C
60.86
@Pressure 14.5 psi,
Temperature 176 °F
 63.73
@Pressure 0.100 MPa,
Temperature 70.0 °C
63.73
@Pressure 14.5 psi,
Temperature 158 °F
 66.73
@Pressure 0.100 MPa,
Temperature 60.0 °C
66.73
@Pressure 14.5 psi,
Temperature 140 °F
 69.88
@Pressure 0.100 MPa,
Temperature 50.0 °C
69.88
@Pressure 14.5 psi,
Temperature 122 °F
 73.17
@Pressure 0.100 MPa,
Temperature 40.0 °C
73.17
@Pressure 14.5 psi,
Temperature 104 °F
 76.6
@Pressure 0.100 MPa,
Temperature 30.0 °C
76.6
@Pressure 14.5 psi,
Temperature 86.0 °F
 80.2
@Pressure 0.100 MPa,
Temperature 20.0 °C
80.2
@Pressure 14.5 psi,
Temperature 68.0 °F
 83.96
@Pressure 0.100 MPa,
Temperature 10.0 °C
83.96
@Pressure 14.5 psi,
Temperature 50.0 °F
 87.9
@Pressure 0.100 MPa,
Temperature 0.000 °C
87.9
@Pressure 14.5 psi,
Temperature 32.0 °F
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 333.5 J/g143.5 BTU/lb
Heat of Vaporization 2257 J/g970.9 BTU/lb
 2258 J/g971.3 BTU/lb
CTE, linear  -23.0 µm/m-°C
@Temperature 0.000 °C
-12.8 µin/in-°F
@Temperature 32.0 °F
 29.3 µm/m-°C
@Temperature 10.0 °C
16.3 µin/in-°F
@Temperature 50.0 °F
 69.0 µm/m-°C
@Temperature 20.0 °C
38.3 µin/in-°F
@Temperature 68.0 °F
 153 µm/m-°C
@Temperature 50.0 °C
85.0 µin/in-°F
@Temperature 122 °F
 250 µm/m-°C
@Temperature 100 °C
139 µin/in-°F
@Temperature 212 °F
Specific Heat Capacity 1.867 J/g-°C
@Temperature 25.0 °C
0.4462 BTU/lb-°F
@Temperature 77.0 °F
Vapor
 4.178 J/g-°C
@Pressure 0.100 MPa,
Temperature 30.0 °C
0.9987 BTU/lb-°F
@Pressure 14.5 psi,
Temperature 86.0 °F
CP
 4.179 J/g-°C
@Pressure 0.100 MPa,
Temperature 40.0 °C
0.9987 BTU/lb-°F
@Pressure 14.5 psi,
Temperature 104 °F
CP
 4.181 J/g-°C
@Pressure 0.100 MPa,
Temperature 50.0 °C
0.9992 BTU/lb-°F
@Pressure 14.5 psi,
Temperature 122 °F
CP
 4.182 J/g-°C
@Pressure 0.100 MPa,
Temperature 20.0 °C
0.9995 BTU/lb-°F
@Pressure 14.5 psi,
Temperature 68.0 °F
CP
 4.184 J/g-°C
@Pressure 0.100 MPa,
Temperature 60.0 °C
1.000 BTU/lb-°F
@Pressure 14.5 psi,
Temperature 140 °F
CP
 4.189 J/g-°C
@Pressure 0.100 MPa,
Temperature 70.0 °C
1.001 BTU/lb-°F
@Pressure 14.5 psi,
Temperature 158 °F
CP
 4.192 J/g-°C
@Pressure 0.100 MPa,
Temperature 10.0 °C
1.002 BTU/lb-°F
@Pressure 14.5 psi,
Temperature 50.0 °F
CP
 4.196 J/g-°C
@Pressure 0.100 MPa,
Temperature 80.0 °C
1.003 BTU/lb-°F
@Pressure 14.5 psi,
Temperature 176 °F
CP
 4.205 J/g-°C
@Pressure 0.100 MPa,
Temperature 90.0 °C
1.005 BTU/lb-°F
@Pressure 14.5 psi,
Temperature 194 °F
CP
 4.216 J/g-°C
@Pressure 0.100 MPa,
Temperature 100 °C
1.008 BTU/lb-°F
@Pressure 14.5 psi,
Temperature 212 °F
CP
 4.218 J/g-°C
@Pressure 0.100 MPa,
Temperature 0.000 °C
1.008 BTU/lb-°F
@Pressure 14.5 psi,
Temperature 32.0 °F
CP
Thermal Conductivity  0.0187 W/m-K
@Temperature 26.9 °C
0.130 BTU-in/hr-ft²-°F
@Temperature 80.3 °F
gas at saturation vapor pressure
 0.1317 W/m-K
@Temperature -73.1 °C
0.9140 BTU-in/hr-ft²-°F
@Temperature -99.7 °F
gas at saturation vapor pressure
 0.0271 W/m-K
@Pressure 0.100 MPa,
Temperature 127 °C
0.188 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 260 °F
gas
 0.0357 W/m-K
@Pressure 0.100 MPa,
Temperature 227 °C
0.248 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 440 °F
gas
 0.0471 W/m-K
@Pressure 0.100 MPa,
Temperature 327 °C
0.327 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 620 °F
gas
 0.561 W/m-K
@Pressure 0.100 MPa,
Temperature 0.000 °C
3.89 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 32.0 °F
liquid
 0.580 W/m-K
@Pressure 0.100 MPa,
Temperature 10.0 °C
4.03 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 50.0 °F
liquid
 0.5984 W/m-K
@Pressure 0.100 MPa,
Temperature 20.0 °C
4.153 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 68.0 °F
liquid
 0.6154 W/m-K
@Pressure 0.100 MPa,
Temperature 30.0 °C
4.271 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 86.0 °F
liquid
 0.6305 W/m-K
@Pressure 0.100 MPa,
Temperature 40.0 °C
4.376 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 104 °F
liquid
 0.6435 W/m-K
@Pressure 0.100 MPa,
Temperature 50.0 °C
4.466 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 122 °F
liquid
 0.6543 W/m-K
@Pressure 0.100 MPa,
Temperature 60.0 °C
4.541 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 140 °F
liquid
 0.6631 W/m-K
@Pressure 0.100 MPa,
Temperature 70.0 °C
4.602 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 158 °F
liquid
 0.670 W/m-K
@Pressure 0.100 MPa,
Temperature 80.0 °C
4.65 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 176 °F
liquid
 0.6753 W/m-K
@Pressure 0.100 MPa,
Temperature 90.0 °C
4.687 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 194 °F
liquid
 0.6791 W/m-K
@Pressure 0.100 MPa,
Temperature 100 °C
4.713 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 212 °F
liquid
Melting Point 0.000 °C32.0 °F
Boiling Point 100 °C212 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index  1.31783
@Temperature 100 °C,
Wavelength 589.3 nm
1.31783
@Temperature 212 °F,
Wavelength 589.3 nm
Sodium light
 1.33299
@Temperature 20.0 °C,
Wavelength 589.3 nm
1.33299
@Temperature 68.0 °F,
Wavelength 589.3 nm
Sodium light
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter18.3036
Antoine's Vapor Pressure B Parameter3816.44
Antoine's Vapor Pressure C Parameter-46.13
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
CAS registry number (CARN)7732-18-5
Chemical FormulaH2O
Critical Compressibility (Zc)0.229
Dipole moment (p/C.m)6.004E-28
Dynamic Viscosity Formulalog10 η=A(1/T-1/B)
Dynamic Viscosity Parameter A658.25
Dynamic Viscosity Parameter B283.16
Molar Heat Capacity (298K)33.637 J/mol-K
Molar Heat Capacity of Vapor a Parameter32.221
Molar Heat Capacity of Vapor b Parameter0.0019
Molar Heat Capacity of Vapor c Parameter1.055E-05
Molar Heat Capacity of Vapor d Parameter-3.594E-09
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K
UV cut-off (nm)191

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Whole Blood
Ice
Aluminum 6061-T6; 6061-T651
Ethylene glycol, C2H6O2
Copper, UNS C12000

DWATR0 / 3094

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.