MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Ineos H04W-01 PP Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Product Description: H04W-01 is a homopolymer polypropylene designed for extrusion processing in applications that require low water-carry-over. Typical applications include Carpet Backing, Woven Bags, and Twine.
Availability: North America
Features: Food Contact Acceptable; Homopolymer; Low Water Carryover
Uses: Bags; Carpet Backing; Twine
Agency Rating: EC 1907/2006 (REACH) ; FDA 21 CFR 177.1520© 3.1a
RoHS Compliance: Contact Manufacture
Forms: Pellets
Processing Method: Extrusion

Information provided by INEOS Olefins & Polymers USA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.908 g/cc0.0328 lb/in³ASTM D792
Melt Flow 4.2 g/10 min
@Load 2.16 kg,
Temperature 230 °C
4.2 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 103103Injection Molded; ASTM D785
Tensile Strength at Break 18.1 MPa2630 psi2.0 in/min, Injection Molded; ASTM D638
Tensile Strength, Yield 36.2 MPa5250 psi2.0 in/min, Injection Molded; ASTM D638
Elongation at Break 150 %150 %2.0 in/min, Injection Molded; ASTM D638
Elongation at Yield 9.5 %9.5 %2.0 in/min, Injection Molded; ASTM D638
Flexural Modulus, 1% Secant 1650 MPa239000 psiInjection Molded; ASTM D790A
Izod Impact, Notched 0.374 J/cm0.700 ft-lb/inInjection Molded; ASTM D256
Izod Impact, Notched (ISO) 3.59 kJ/m²1.71 ft-lb/in²Area, Injection Molded; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 106 °C223 °FUnannealed, Injection Molded; ASTM D648
 
Optical PropertiesMetricEnglishComments
Haze 78.8 %
@Thickness 1.27 mm
78.8 %
@Thickness 0.0500 in
Injection Molded; ASTM D1003
Gloss 92 %92 %60°, Injection Molded; ASTM D2457
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PINEOSA012 / 268248

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.