MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AGC ASAHIKLIN AK-225AES Hydrochlorofluorocarbon Solvent
Categories: Fluid; Solvent

Material Notes: AK-225 AES was developed as a defluxing agent. It is an azeotrope-like mixture of AK-225, ethanol and stabilizer and is suitable for use in a vapor degreaser. It effectively removes flux residues as well as ionic soils from printed circuit boards and other electronic devices. AK-225 is exempt from VOC regulations by the U.S. EPA as described in the Oct. 8, 1996 Federal Register.

Information provided by Asahi Glass Company, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.49 g/cc
@Temperature 25.0 °C
Liquid
Solubility of Water 0.33 %25°C
Solubility in Water 0.053 %25°C
Viscosity 0.61 cP
@Temperature 25.0 °C
Vapor Pressure 0.388 bar
@Temperature 25.0 °C
Surface Tension 16.8 dynes/cm25°C
 
Thermal PropertiesOriginal ValueComments
Heat of Vaporization 40.6 cal/gb.p.
Specific Heat Capacity 1.13 J/g-°C
Melting Point -138 °C
Boiling Point 52.0 °C
 
Descriptive Properties
KB Value41
Relative Evaporation Rate (ether=100)81

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WAGC03 / 74559

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.