PC+ABS)-Blend; flame retardant; easy flowing; for high gloss applications; RHCM process etc.; Vicat/B 120 temperature = 96 °C; UL recognition 94 V-0 at 1.2 mmAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |