MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Riteflex® 655HS TPC, Unfilled
Categories: Polymer; Thermoplastic; Polyester, TP; Polyester Thermoplastic Elastomer

Material Notes: 55 Shore D Hardness heat stabilized

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Density 1.19 g/ccISO 1183
Water Absorption 0.40 %
@Temperature 22.8 °C
24hr immersion; ASTM D570
Linear Mold Shrinkage, Flow 0.010 cm/cmASTM D955
 0.016 - 0.019 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.017 - 0.021 cm/cmISO 294-4
Melt Flow 9.0 g/10 min
@Load 2.16 kg,
Temperature 220 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 55ASTM D2240
Tensile Strength at Break 3800 psiASTM D638
Elongation at Break 330 %ASTM D638
Flexural Strength 7.00 MPa
@Strain 3.5 %
ISO 178
Flexural Modulus 205 MPaISO 178
 30000 psiASTM D790
Izod Impact, Notched 99.0 ft-lb/inASTM D256
Charpy Impact Unnotched NBISO 179/1eU
Charpy Impact, Notched 65.0 kJ/m²partial break; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.00e+12 ohm-cmASTM D257
 2.00e+15 ohm-cmIEC 60093
Dielectric Constant 4.0
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 14.0 kV/mmIEC 60243-1
 350 V/milshort term; ASTM D149
Dissipation Factor 0.040
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index >= 600 VASTM D3638
 >= 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 392 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °CISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °CISO 75-1, -2
Vicat Softening Point 352 °FASTM D1525
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Processing Temperature 20.0 - 55.0 °Ccavity
 205 - 235 °Chot runner
Feed Temperature 200 - 215 °C
Zone 1 200 - 215 °C
Zone 2 205 - 230 °C
Zone 3 205 - 230 °C
Zone 4 205 - 235 °C
Die Temperature 205 - 235 °C
Melt Temperature 205 - 235 °C
Drying Temperature 100 - 110 °C
Dry Time 4.00 hour
Moisture Content <= 0.050 %
 
Descriptive Properties
Injection speedmedium-fast
Processing typeInj/Blow/Ext

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Riteflex® 655A TPC, Unfilled
Celanese Riteflex® 640A TPC, Unfilled
Celanese Riteflex® 440 TPC, Unfilled
Celanese Riteflex® 663 TPC, Unfilled
Celanese Riteflex® 672 TPC, Unfilled

PHCQ453 / 178908

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.