MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Chevron Phillips Marlex® 4553 Polyethylene; LDPE  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Low density polyethylene. This LDPE is tailored for cast film applications that require:
  • High speed extrusion
  • Low neck-in
  • Good drawdown
  • Edge tear resistance
  • Low coefficient of friction

Applications: Typical cast film applications include:

  • Personal care
  • General purpose

Information provided by Phillips

Formerly branded with the MarFlex® trade name.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.924 g/ccASTM D-1505
Water Vapor Transmission 13.0 g/m²/dayCast Film at 1.25 mil; ASTM F-1249
Oxygen Transmission Rate 6200 cc/m²/dayCast Film at 1.25 mil; ASTM D-3985
Melt Index of Compound 4.1 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D-1238
Antiblock Level 0.00 ppm
Slip Level 650 ppm
 
Mechanical PropertiesOriginal ValueComments
Coefficient of Friction 0.13Cast Film at 1.25 mil; ASTM D-1894
Elmendorf Tear Strength, MD 320 g/milCast Film at 1.25 mil; ASTM D-1922
Elmendorf Tear Strength, TD 125 g/milCast Film at 1.25 mil; ASTM D-1922
Dart Drop 65.0 g/milCast Film at 1.25 mil; ASTM D-1709
 
Thermal PropertiesOriginal ValueComments
Melting Point 109 °CASTM D-3418
Vicat Softening Point 99.0 °CASTM D-1525
 
Optical PropertiesOriginal ValueComments
Haze 9.5 %
@Thickness 0.0317 mm
Cast Film; ASTM D-1003
Gloss 84 %60°, Cast Film at 1.25 mil; ASTM D-2457

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® 1003 LDPE Injection Molding Resin
Chevron Phillips Marlex® 1122B Injection Molding Resin
Chevron Phillips Marlex® 1412 Injection Molding Resin
Chevron Phillips KN 230B LDPE Injection Molding Resin
Chevron Phillips 5102 LDPE Injection Blow Molding Resin

PCHEVD224 / 20718

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.