MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Michelman® VaporBase™ 1065 MVTR primer  (discontinued **)
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: MVTR primer

Usage: VaporBase™ 1065 is a primer designed to be used in tandem with the VaporCoat® series of products. VaporBase™ 1065 works to seal the base substrate allowing the top coat to work more efficiently for best MVTR.

Application Data: VaporBase™ 1065 is typically applied by rod coater.

Common uses include: Roll wrap for fine papers; Produce and poultry boxes; Frozen meat patty boxes; and Archival storage

Food Contact Information when manufactured in the USA:
FDA:
175.105: Components of adhesives.
176.170: Components of paper and paperboard in contact with aqueous and fatty foods(Restricted).
176.180: Components of paper and paperboard in contact with dry foods.

Food Contact Information when manufactured in Singapore:
FDA:
175.105: Components of adhesives.
176.170: Components of paper and paperboard in contact with aqueous and fatty foods(Restricted).
176.180: Components of paper and paperboard in contact with dry foods. (Restricted)

Information provided by Michelman®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.27 - 1.29 g/cc1.27 - 1.29 g/cc
pH 7.0 - 9.07.0 - 9.0
Brookfield Viscosity 150 - 400 cP150 - 400 cPSpindle # 3, rpm 60
Viscosity Measurement 10 - 1510 - 15[sec], EZ cup, Cup # 3
 
Descriptive Properties
AppearanceCream colored, semi-translucent liquid
Solids TypePolymer

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WMICHEL203 / 135120

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.