Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Filler/Reinforcement: Glass Fiber, 30% Filler by Weight Features: High Heat Resistance; Hydrolysis Resistant Uses: Automotive Applications; Automotive Exterior Parts; Automotive Interior Parts; Consumer Applications; Hydraulic Applications; Industrial Applications; Pneumatic Applications RoSH Compliance: RoSH Compliant Automotive Specifications: GM GMW15702-013082 PPA-GF30 Appearance: Black Forms: Granules Processing Method: Injection Molding Information provided by EMS-Grivory |