MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

CHT SilSo SE2014 Silicone elastomer
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: This is a 2-component, silicone elastomer system specially designed for electronic potting and encapsulation applications. It offers good protection against chemicals, environmental contamination, mechanical shock, vibration and impact damage. It can be employed in areas where low flammability is a prerequisite. The cured elastomer can be repaired. The component parts have relatively low viscosities and are readily mixed either by hand or machine.

Key Features

  • Light weight and low density
  • Long pot life
  • UL recognized in file number E334038
  • Very high dielectric strength
Application: Coating for the umbilical cable ROV underwater remotely operated vehicles

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.730 g/cc0.0264 lb/in³Cured Product; BS ISO 2781
 0.770 g/cc0.0278 lb/in³B; BS ISO 2781
 0.790 g/cc0.0285 lb/in³A; BS ISO 2781
Brookfield Viscosity 7200 cP7200 cPB
 10000 cP10000 cPMixed
 12200 cP12200 cPA
Storage Temperature <= 30.0 °C<= 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6767ASTM D2240-95
Tensile Strength 2.70 MPa392 psiISO 37
Elongation at Break 54 %54 %ISO 37
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D-257
Dielectric Constant 2.292.29ASTM D-150
Dielectric Strength 32.1 kV/mm816 kV/inASTM D-149
Dissipation Factor 0.001740.00174ASTM D-150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 218 µm/m-°C121 µin/in-°F
Thermal Conductivity 0.140 W/m-K0.972 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 200 °C392 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Processing PropertiesMetricEnglishComments
Pot Life 360 min360 min
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AppearanceViscous liquid
ColorGreenB
 GreenCured Product
 Off whiteA
Cure typeAddition
Mix Ratio1:1By Weight
RheologyLiquid
Self BondingNo
Volume Coefficient of Thermal Expansion818 ppm/°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHTSIL065 / 314548

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.