MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
CHT Group QM 140 QSI Quantum Silicones 40 Durometer Condensation Cured Moldmaking Material
Categories: Polymer; Thermoset; Silicone

Material Notes: QM 140 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent choice for the molding of intricate patterns, skin molding and applications where high durometer, dimensional stability and extremely tough rubber are required. Complies with FDA indirect food contact regulation CFR 177.2600 when used with Cat Clear FG. Refer to Cat Clear FG data sheet for specific properties.

Key Features:

  • Low viscosity
  • High tear strength
  • Fast demold time
  • Excellent dimensional stability
Main Applications:
  • Molds for polyester, polyurethane and epoxy resin castings
  • Molds for technical articles and prototype
  • Molds for furniture and picture frame replication

      Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.03 g/ccUncatalyzed, QM CAT 140
 1.13 g/cccatalyzed with QM CAT Clear FG
 1.16 g/ccBase
 1.31 g/cccatalyzed with QM CAT 140
Viscosity 250 cPUncatalyzed, QM CAT 140
 3700 cPcatalyzed with QM CAT Clear FG
 37000 cPcatalyzed with QM CAT 140
 50000 cPBase
Linear Mold Shrinkage <= 0.0030 cm/cmcured 72 hrs @ RT, w/ QM Cat 140
 <= 0.0030 cm/cmcured 72 hrs @ RT, w/ QM Cat Clear FG
Storage Temperature <= 38.0 °C6 months
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 30cured 72 hrs @ RT, w/ QM Cat Clear FG
 40cured 72 hrs @ RT, w/ QM Cat 140
Tensile Strength 4.50 MPacured 72 hrs @ RT, w/ QM Cat 140
 650 psicured 72 hrs @ RT, w/ QM Cat Clear FG
Elongation at Break 300 %cured 72 hrs @ RT, w/ QM Cat 140
 530 %cured 72 hrs @ RT, w/ QM Cat Clear FG
Tear Strength 160 pliB, cured 72 hrs @ RT, w/ QM Cat 140
 160 plicured 72 hrs @ RT, w/ QM Cat Clear FG
 
Processing PropertiesOriginal ValueComments
Cure Time 12 - 16 hourDemold time, catalyzed with QM CAT 140
 12.0 - 16.0 hourDemold time, catalyzed with QM CAT Clear FG
Tack-Free Time 4.00 - 6.00 hourCatalyzed with QM CAT 140
 4.00 - 6.00 hourCatalyzed with QM CAT Clear FG
Pot Life 45.0 mincatalyzed with QM CAT 140
 45.0 mincatalyzed with QM Clear FG
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
ColorBeigeBase
 Beigecatalyzed with QM Clear FG
 Light Purple catalyzed with QM CAT 140
 PurpleUncatalyzed, QM CAT 140

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CHT Group QSil 551 QSI Quantum Silicones Silicone Potting Material
CHT Group QM 245 QSI Quantum Silicones 45 Durometer Addition Cure Moldmaking Material
CHT Group MM940 Condensation Cure 2-Part Molding Rubber
CHT Group QLE 1020 QSI Quantum Silicones 45 Durometer Clear, Addition Cure Elastomer for Coating
CHT Group QLE 1039 QSI Quantum Silicones 40 Durometer Addition Cure Elastomer for Coating

PACC061 / 22188

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.