System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Ovako S235JR SS 14 13 12:1987 (ref) Steel, +AR
Categories:
Metal
;
Ferrous Metal
;
Alloy Steel
Material Notes:
General Information:
Soft structural steel easy to weld and bend.
Information provided by Ovako
Key Words:
SS 1312, S235JR, 1.0038, Fe 360 BFN, RSt37-2, 40 B
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
7.80
g/cc
Mechanical Properties
Original Value
Comments
Hardness, Brinell
<= 130
@Thickness <=40.0 mm
All formats
<= 130
@Thickness 40.1 - 100 mm
All formats
Tensile Strength
360
-
460
MPa
@Thickness <=40.0 mm
All formats
360
-
460
MPa
@Thickness 40.1 - 100 mm
All formats
Tensile Strength, Yield
>=
230
MPa
@Thickness 40.1 - 100 mm
R
eh
, All formats
>=
240
MPa
@Thickness <=40.0 mm
R
eh
, All formats
Elongation at Break
25 %
@Thickness <=40.0 mm
All formats
25 %
@Thickness 40.1 - 100 mm
All formats
Modulus of Elasticity
210
GPa
Poissons Ratio
0.30
Shear Modulus
80.0
GPa
Electrical Properties
Original Value
Comments
Electrical Resistivity
0.00000200
-
0.00000250
ohm-cm
Thermal Properties
Original Value
Comments
CTE, linear
12.0
µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity
0.460
-
0.480
J/g-°C
@Temperature 50.0 - 100 °C
Thermal Conductivity
40.0
-
45.0
W/m-K
Ambient temperature
Transformation Temperature
485
°C
MS
725
°C
AC1
863
°C
AC3
Component Elements Properties
Original Value
Comments
Carbon, C
<= 0.20 %
Iron, Fe
>= 99.69 %
As Balance
Nitrogen, N
<= 0.012 %
Phosphorus, P
<= 0.050 %
Sulfur, S
<= 0.050 %
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Ovako S235JR EN10025-2 (ref) Steel, +AR
EN S235JR High Manganese, Structural, Hot Rolled, Base Steel, t < 16 mm
ASTM A284 Steel, grade C
EN S235JR Structural, Hot Rolled, Base Steel, 16 mm < t < 25 mm
ASTM A284 Steel, grade D
NOVAKO409 / 234708
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.