MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Solvay MIRACARE® PS Surfactant  (discontinued **)
Categories: Fluid

Material Notes: Description: Formulated surfactant concentrate used in the preparation of high foaming pearlized shampoos, body washes, and liquid handsoaps.

C.T.F.A. / I.N.C.I. Name: WATER (AND) SODIUM LAURETH SULFATE (AND) SODIUM COCOAMPHOACETATE (AND) COCAMIDE MIPA (AND) PROPYLENE GLYCOL (AND) GLYCOL DISTEARATE

CAS: 7732 – 18 – 5 / 68585 – 34 – 2 / 68608 – 65 – 1 / 68333 – 82 – 4 / 57 – 55 – 6 / 627 – 83 – 8

Available in: Asia Pacific, Europe, Latin America and North America

Solubility: Water (in all proportions

Applications: MIRACARE PS was specially designed for easy-to-formulate, cold process pearlescent shampoos and shower gels for adults. MIRACARE PS is compatible with most conditioning agents, (such as MIRAPOL A 15, MIRAPOL 550 and JAGUAR C 162) allowing to formulate easily 2 in 1 shampoos and shower gels. MIRACARE PS can be diluted in water: at ratios 1:5 for economical shampoos at ratios of 1:3 for premium mild shampoos and shower gels. MIRACARE PS provides a rich creamy flash lather.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
pH 5.0 - 7.05.0 - 7.0540MA3C1E
Viscosity <= 4000 cP<= 4000 cP540MO3C16
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 59 - 63 %59 - 63 %Karl Fischer; 540MAC1C
 
Descriptive Properties
ColorPearly Ivory
CompositionActive37-41%
 Propylene Glycol<6%
PreservativeDiazoldnyl Urea
 Methylparaben
 Propylparaben
Setting point5°C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WRHOD248 / 137479

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.