MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Carpenter AerMet® 340
Categories: Metal; Ferrous Metal; Alloy Steel; Tool Steel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.86 g/cc0.284 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 2430 MPa352000 psi
Tensile Strength, Yield 2160 MPa314000 psi
Elongation at Break 11.3 %11.3 %
Reduction of Area 55.2 %55.2 %
Tensile Modulus 192 GPa27900 ksi
Fatigue Strength 986 MPa
@# of Cycles 1.00e+7
143000 psi
@# of Cycles 1.00e+7
R=-1, Kt=1
Fracture Toughness 34.61 MPa-m½31.50 ksi-in½
Charpy Impact 14.6 J10.8 ft-lbnotched

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carpenter AerMet® 310
Carpenter AerMet® 100 Aged at 875°F
QuesTek® Innovations Ferrium® M54™ Ultrahigh-strength Steel for Structural Applications
Carpenter AerMet® 100 Aged at 900°F
Latrobe Lescalloy® 300M - HS VAC-ARC High Strength Alloy Steel

NCARL5 / 15806

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.