MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Telles Mirel™ I6001 Biobased Polymeric Modifier
Categories: Polymer; Renewable/Recycled Polymer

Material Notes: I6001 is an effective multifunctional, >85% biobased polymeric modifier for semi-rigid and flexible PVC compounds. It improves impact resistance, tear resistance, tensile toughness and plasticization, while not compromising clarity or UV stability. It also promotes shear melting and faster fusion giving processing advantages over traditional core-shell impact modifiers. This multifunctional modifier allows the overall formulation to be simplified and the additives package to be cost effectively rebalanced. This product is ideal for applications requiring very low migration, extraction and VOC formation for applications in the automotive, medical, packaging and construction industries.

Telles is a joint venture between Metabolix and Archer Daniels Midland Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/cc
Bulk Density 0.500 g/cc0.0181 lb/in³
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -8.00 - -2.00 °C17.6 - 28.4 °F
 
Processing PropertiesMetricEnglishComments
Drying Temperature 80.0 °C
@Time 14400 sec
176 °F
@Time 4.00 hour
if necessary
Moisture Content <= 0.050 %<= 0.050 %
 
Descriptive Properties
ColorOff White
FormPellets80% < 2 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Telles Mirel™ P1003 Injection Molding Grade PHA Bioplastic
Telles Mirel™ I6003rp Biobased PHA Polymeric Modifier
Geon® Performance Solutions Vinyl Wire & Cable W1201 Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Flexible XV3715 Polyvinyl Chloride, Flexible
FKuR Kunststoff Terralene® LL 1303 Biobased Polyethylene

PMETAA960 / 108488

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.