MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Sarlink® TPE ME-2350B BLK Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Sarlink ME-2350B BLK is a high performance thermoplastic elastomer designed for automotive exterior application with good UV resistance and good flow properties.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Good Flow; Low Density; UV Resistant

Uses: Automotive Applications; Automotive Exterior Parts

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.903 g/cc0.0326 lb/in³ASTM D792
Viscosity 126 cP
@Shear Rate 206 1/s,
Temperature 200 °C
126 cP
@Shear Rate 206 1/s,
Temperature 392 °F
ASTM D3835
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
7.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5050ASTM D2240
Tensile Strength at Break 9.58 MPa1390 psiASTM D412
Tensile Stress at Strain 1.20 MPa
@Strain 100 %
174 psi
@Strain 100 %
ASTM D412
Elongation at Break 930 %930 %ASTM D412
Compression Set 41 %
@Temperature 70.0 °C,
Time 79200 sec
41 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 199 - 210 °C390 - 410 °F
Middle Barrel Temperature 204 - 216 °C400 - 420 °F
Front Barrel Temperature 210 - 221 °C410 - 430 °F
Nozzle Temperature 216 - 227 °C420 - 440 °F
Melt Temperature 216 - 227 °C420 - 440 °F
Mold Temperature 35.0 - 65.6 °C95.0 - 150 °F
Injection Pressure 1.38 - 6.89 MPa200 - 1000 psi
Back Pressure 0.172 - 0.862 MPa25.0 - 125 psi
Cushion 0.381 - 2.54 cm0.150 - 1.00 in
Screw Speed 50 - 120 rpm50 - 120 rpm
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Dynaflex™ G7950-1001-00 Thermoplastic Elastomer (TPE)
Teknor Apex Sarlink® TPE OM-1150N Thermoplastic Elastomer
Teknor Apex Sarlink® TPE ML-1650N NAT Thermoplastic Elastomer
Teknor Apex Sarlink® TPE ML-1150N NAT Thermoplastic Elastomer
Teknor Apex Sarlink® TPE ME-2255B Thermoplastic Elastomer

PTEKNQ1069 / 237560

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.