MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

CHT AS1421 1-part, silicone adhesive sealant
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: This is a heat cured, non-corrosive, neutral cure, 1-part, silicone adhesive sealant. It is one in a range of Addition cure products which are solvent free. It exhibits primerless adhesion to many substrates when cured at temperatures above 100°C. It cures to form a very tough resilient silicone elastomer. This product will not corrode copper or its alloys and is suitable for use with electronic components.

Key Features

  • UL94 V0 recognized in file No. E334038
  • Excellent thermal conductivity
  • Fast heat cure
  • Adhesion to most substrates
Application: Electronics

Cured Product: After 1 hour at 125°C

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.18 g/cc0.0788 lb/in³BS ISO 2781
Brookfield Viscosity 140000 - 240000 cP140000 - 240000 cPMixed
Storage Temperature -5.00 - 10.0 °C23.0 - 50.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5656ASTM D2240-95
Tensile Strength 2.20 MPa319 psiISO 37
Elongation at Break 105 %105 %ISO 37
Tensile Modulus 0.000752 GPa0.109 ksiYoung's
Shear Strength 0.753 MPa109 psiLap Shear Aluminum; ASTM D1002
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.50e+13 ohm-cm3.50e+13 ohm-cmASTM D-257
Dielectric Strength >= 18.0 kV/mm>= 457 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 195 µm/m-°C108 µin/in-°F
Thermal Conductivity 2.10 W/m-K14.6 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 210 °C410 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 16.0 min
@Temperature 100 °C
0.267 hour
@Temperature 212 °F
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AppearanceGrey paste
ColorGrey
Cure typeAddition Heat Cure
RheologyPaste
Self BondingYes
Volume Coefficient of Thermal Expansion586 ppm/°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHTSIL007 / 314490

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.